Hydrolytic and enzymatic degradation studies of aliphatic 10-undecenoic acid-based polyesters

  • Dades identificatives

    Identificador: imarina:5132960
    Autors:
    Valverde C., Lligadas G., Ronda J., Galià M., Cádiz V.
    Resum:
    The hydrolytic and enzymatic degradations of aliphatic polyesters: poly (10,11-epoxyundecanoic acid) (PEAU) bearing hydroxyl groups along the main chain and poly (11-hydroxyundecanoate)diol (PHU), were studied and compared to that of commercial poly (ε-caprolactone)diol (PCL). Changes taking place after polyester degradation in sample weight, molecular weight (Mn), chemical constitution, thermal properties, crystallinity and morphology were monitored by size exclusion chromatography (SEC), 1H nuclear magnetic resonance (NMR) spectroscopy, differential scanning calorimetry (DSC), thermogravimetric analysis (TGA), X-Ray diffraction (XRD) and environmental scanning electron and atomic force microscopies (ESEM and AFM). A significant decrease of PEUA Mn in both hydrolytic and enzymatic degradation was detected versus PHU and PCL, and related to its hydrophilic character, by the presence of hydroxyl pendant groups, and the superior amorphous character. An accelerated degradation in acidic media, monitored by SEC and 1H NMR spectroscopy to study in detail all residual material of three polyesters, showed the complete degradation only in the case of PEUA and PCL.
  • Altres:

    Autor segons l'article: Valverde C., Lligadas G., Ronda J., Galià M., Cádiz V.
    Departament: Química Analítica i Química Orgànica
    Autor/s de la URV: Cádiz Deleito, Maria Virginia / Galià Clua, Marina Teresa / Lligadas Puig, Gerard / Ronda Bargalló, Juan Carlos
    Paraules clau: Hydrolytic degradation Enzymatic degradation Biobased Aliphatic polyesters
    Resum: The hydrolytic and enzymatic degradations of aliphatic polyesters: poly (10,11-epoxyundecanoic acid) (PEAU) bearing hydroxyl groups along the main chain and poly (11-hydroxyundecanoate)diol (PHU), were studied and compared to that of commercial poly (ε-caprolactone)diol (PCL). Changes taking place after polyester degradation in sample weight, molecular weight (Mn), chemical constitution, thermal properties, crystallinity and morphology were monitored by size exclusion chromatography (SEC), 1H nuclear magnetic resonance (NMR) spectroscopy, differential scanning calorimetry (DSC), thermogravimetric analysis (TGA), X-Ray diffraction (XRD) and environmental scanning electron and atomic force microscopies (ESEM and AFM). A significant decrease of PEUA Mn in both hydrolytic and enzymatic degradation was detected versus PHU and PCL, and related to its hydrophilic character, by the presence of hydroxyl pendant groups, and the superior amorphous character. An accelerated degradation in acidic media, monitored by SEC and 1H NMR spectroscopy to study in detail all residual material of three polyesters, showed the complete degradation only in the case of PEUA and PCL.
    Àrees temàtiques: Química Polymers and plastics Polymer science Odontología Mechanics of materials Materials chemistry Materiais Interdisciplinar Farmacia Engenharias ii Engenharias i Condensed matter physics Ciências biológicas ii Ciências biológicas i Ciências ambientais Ciências agrárias i Biotecnología Astronomia / física Arquitetura e urbanismo
    ISSN: 01413910
    Adreça de correu electrònic de l'autor: marina.galia@urv.cat juancarlos.ronda@urv.cat gerard.lligadas@urv.cat
    Identificador de l'autor: 0000-0002-4359-4510 0000-0002-0668-6600 0000-0002-8519-1840
    Data d'alta del registre: 2024-09-07
    Versió de l'article dipositat: info:eu-repo/semantics/acceptedVersion
    Enllaç font original: https://www.sciencedirect.com/science/article/pii/S0141391018302234
    URL Document de llicència: https://repositori.urv.cat/ca/proteccio-de-dades/
    Referència a l'article segons font original: Polymer Degradation And Stability. 155 84-94
    Referència de l'ítem segons les normes APA: Valverde C., Lligadas G., Ronda J., Galià M., Cádiz V. (2018). Hydrolytic and enzymatic degradation studies of aliphatic 10-undecenoic acid-based polyesters. Polymer Degradation And Stability, 155(), 84-94. DOI: 10.1016/j.polymdegradstab.2018.07.012
    DOI de l'article: 10.1016/j.polymdegradstab.2018.07.012
    Entitat: Universitat Rovira i Virgili
    Any de publicació de la revista: 2018
    Tipus de publicació: Journal Publications
  • Paraules clau:

    Condensed Matter Physics,Materials Chemistry,Mechanics of Materials,Polymer Science,Polymers and Plastics
    Hydrolytic degradation
    Enzymatic degradation
    Biobased
    Aliphatic polyesters
    Química
    Polymers and plastics
    Polymer science
    Odontología
    Mechanics of materials
    Materials chemistry
    Materiais
    Interdisciplinar
    Farmacia
    Engenharias ii
    Engenharias i
    Condensed matter physics
    Ciências biológicas ii
    Ciências biológicas i
    Ciências ambientais
    Ciências agrárias i
    Biotecnología
    Astronomia / física
    Arquitetura e urbanismo
  • Documents:

  • Cerca a google

    Search to google scholar